Injection molding process to enhance PA66 and reduce floating fibers in PA6


First is the barrel temperature. Since the melt flow rate of glass fiber reinforced plastics is 30% to 70% lower than that of non-reinforced plastics, their fluidity is poorer. Therefore, the barrel temperature should be 10 to 30°C higher than usual. Increasing the barrel temperature can reduce the melt viscosity, improve fluidity, and prevent filling and weld line defects.